I've glassed the hybrid with 4 oz. s-cloth, and sb112 resin from Merton's.  The s-cloth is stronger than regular e-cloth, and the sb112 resin, while expensive (about $100 per board), comes highly recommended.  It bonds with polyester resin with only sanding, and it has uv blocker.  Its a slow setup, 12 hours, accelerated only with heat.  It's purportedly good for lam coat, hot coat, and gloss coat.  